Do you have small or fragile metallic samples and you want to use electrolytic preparation? We will give some tipps for preparing such specimen using electrolytic polishing/ etching equipment.

Watch webinar

Webinaires enregistrés

Electrolytic preparation of small and irregular samples

Do you have small or fragile metallic samples and you want to use electrolytic preparation? We will give some tipps for preparing such specimen using electrolytic polishing/ etching equipment.

Electrolytic preparation offers many possibilities for fast and low-deformation preparation on metallic samples. In some cases, electrolytic preparation is difficult due to sample size or geometry. In this webinar we will give some tips how to prepare such samples.

Information sur ce stage

  • Sujet

    Matérialographie

  • Host

    Dr. Holger Schnarr, spécialiste en applications

  • Langue

    Anglais

  • Disponibilité

    Oui

Lieu et horaires

Information complémentaire