Troubleshooting: Grinding and polishing

Watch webinar

Webinaires enregistrés

Troubleshooting: Grinding and polishing

The seminar will present you for challenges in materialographic grinding and polishing and introduce a guide to find solutions when problems occur. The Webinar will enable you to: - Detect sample effects or damage from mechanical preparation proces - Troubleshoot problems e.g. pencil shape or relief - Overview parameters affecting grinding/polishing result