Materialographic Preparation: 10 Common Mistakes And How To Avoid Them

​Final results in sample preparation can be affected by wrong use of machines and consumables. During this webinar we will go through 10 usual mistakes and we will learn what are their causes, consequences and solutions.

Watch webinar

録画ウェビナ―

Materialographic Preparation: 10 Common Mistakes And How To Avoid Them

​Final results in sample preparation can be affected by wrong use of machines and consumables. During this webinar we will go through 10 usual mistakes and we will learn what are their causes, consequences and solutions.

Materialographic preparation can be tricky. It is a common assumption to believe that using the best cutting and polishing machines or the highest quality resins and diamond suspensions is enough to obtain perfect results. If used wrong, even the most expensive instrument can lead to bad results.

During this webinar, the most common mistakes will be identified and analysed, and simple but effective solutions will be provided.