Preparation Effects on Thermal Spray Coatings

The aim is to show you how to attain improved results of your samples and even in less time. I will guide you through a direct comparison between a typical method in the spray coatings labs and the typical Struers method. For both methods I have used a few coatings and prepared each of them for optical comparison. One of these will be a discussion about preparation of coatings including T-800 low oxide and T-800 high oxide coatings. < br="" />